The microstructure and formation mechanism of the boron carbide (B 4 C) and titanium alloy (TC4) joints brazed with AgCuTi-AlN-W + Mo foil + Nb foil brazing filler were investigated. The effects of W/AlN content on microstructure and mechanical properties of the joints were discussed. To alleviate residual thermal stress, refractory metal foils such as Mo/Nb foils were added. Compared with the common composite interlayers, the interlayer formed via AgCuTi-AlN-W + Mo foil + Nb foil in-situ alloying had more and finer reinforcing phases without reducing the activity of the filler material. The ductile Mo/Nb foils contributed to accommodate the large strain mismatch by elastic deformation. The interfaces between the adjoining materials and the interlayer were well-bonded without any cracks. The most effective system was nickel-plated B 4 C + Mo foil + AgCuTi-3 wt% AlN-5 wt% W + AgCu foil + Nb foil + TC4, which exhibited the highest shear strength of approximately 115 MPa.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: