Answers are grounded in this paper and cite their sources.
In-situ real-time spectroscopic ellipsometry (RTSE) measurements are performed on a growing amorphous vanadium oxide (a-VOx) film to determine the complex dielectric function (ε = ε1 + iε2) spectra, structure, and oxygen content (x) with depth during deposition. VOx with x ∼2 is annealed to produce polycrystalline VO2 and characterized by near-infrared to ultraviolet (0.75 - 5.9 eV) spectroscopic ellipsometry during heating and cooling from room temperature (RT) to 343 K to RT to track hysteresis effects in the semiconducting-to-metal transition (SMT). Spectra in ε are measured for as-deposited and annealed films prepared with varying deposition parameters to determine the as-deposited film x and verify the SMT. Temperature-dependent IR extended spectroscopic ellipsometry is performed from 0.06 - 0.74 eV to determine the IR ε spectra of polycrystalline VO2 across the SMT. As-deposited amorphous VOx films with x from 1.89 ≤ x ≤ 2.14 transition to polycrystalline VO2 after annealing and exhibit the SMT when heated from RT to 343 K which are verified by substantially increased ε2 magnitude at ≥ 343 K. By identifying x of a-VOx from ε spectra, a shortened path of qualifying a-VOx films which will crystallize to phase change VO2 is developed.
No takes yet. Share an insight, caveat, or question.
Jayswal et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: