To address the problems of insufficient strength and low hardness in pure titanium, a new Ti-B-C powder system was used to prepare in-situ hybrid reinforced (TiB+TiC)/Ti composites by laser powder bed fusion (LPBF) technology. The influence of different TiB/TiC ratios on the hybrid reinforcement was investigated. When the TiB/TiC ratio is 1:1, the best hybrid reinforcement effect is achieved and the mechanical interlocking structure is formed between TiB and TiC. The structures enhance the strength of (TiB+TiC)/Ti composites significantly. Subsequently, the microstructures and mechanical properties of (TiB+TiC)/Ti composites were investigated by adjusting different TiB+TiC contents. As the TiB+TiC content increases, the grains are refined significantly and transform into equiaxed grains eventually, the preferred orientation disappears. When the TiB+TiC content is too high, severe agglomeration of TiB+TiC occurs, resulting in less noticeable improvement in strength and a rapid decrease in plasticity. Finally, the heat treatment of (TiB+TiC)/Ti composites was carried out. TiB and TiC are uniformly distributed. TiC coarsens significantly, and TiB exhibits a dual-scale effect. The higher the heat treatment temperature, the more favorable it is to improve the plasticity of titanium matrix composites (TMCs). The TMC2 after HT950 has a tensile strength of 879 MPa and an elongation of 11.7%, exhibiting excellent comprehensive mechanical properties.
No takes yet. Share an insight, caveat, or question.
Wu et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: