This is the authors' abstract. We don't add key points for this paper.
Herein, a mixture of real polypropylene (PP) waste was pyrolyzed with a HZSM-11 catalyst as a potential method to recover light hydrocarbons (C ≤ 12 ), the potential feedstock for value-added chemicals and fuels, from polyolefin plastic waste. Using the HZSM-11 in the PP waste mixture pyrolysis noticeably improved the yield of gas pyrolysate and oil in compensation for the yield of wax (i.e. hydrocarbons of C > 20 ) and solid residue particularly at a higher temperature. In addition, the selectivity of C 3 –C 12 in the PP-waste mixture-derived pyrolysate was markedly increased by the HZSM-11. The highest yield of light hydrocarbons was ≈40 wt% (per mass of the feedstock) achieved at 700 °C with the HZSM-11 catalyst. Despite 7.9 wt% coke deposition on the HZSM-11 after its use in the pyrolysis of the PP waste mixture, the catalyst could be reusable for at least three times after regeneration. The experimental results demonstrate that HZSM-11 has the potential for being a promising catalyst to valorize polyolefin waste into value-added chemicals.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Lee et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: