Answers are grounded in this paper and cite their sources.
An exploration of the plasma-sprayed abradable sealing coatings (ASCs) of a thick and porous LaMgAl11O19 topcoat onto SiC/SiC ceramic matrix composites (CMCs) is detailed in this study. Interlayers comprising Si/Si + Yb2Si2O7/Yb2SiO5 environmental barrier coatings (EBCs) were strategically employed, considering their function in protecting the SiC/SiC CMCs from recession and mitigating thermal expansivity misfit. An isothermal oxidation test was conducted at 1300 °C and resulted in the formation of bubble and glassy melt on the side surface of the coated sample, while a significant reaction layer emerged at the Yb2SiO5/LaMgAl11O19 interface near the edge. The localized temperature rise caused by the exothermic oxidation of the SiC/SiC substrate was determined to be the underlying factor for bubble generation. The temperature-dependent viscosity of the melt contributed to various bubble characteristics, and due to the enrichment of Al ions, the glassy melt exacerbated the degradation of the Yb2SiO5 layer. After a thermal shock test at 1300 °C, the substrate on the uncoated backside of the sample experienced fracture, while the front coating remained intact. However, due to the presence of a through-coating crack, an internal crack network also developed within the substrate.
No takes yet. Share an insight, caveat, or question.
Huang et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: