Residual stress affects the integrity of laser-clad coatings. The aim was to determine how cladding power and scanning speed affect the calculated single-track stress field and how closely regression reproduces local finite element stresses in an Fe-based coating on P20 steel. Sequentially coupled finite element analysis (FEA) transferred the temperature history from a moving Gaussian heat source to an elastic–plastic stress calculation. The predicted fusion boundary was assessed qualitatively against a cross-sectional scanning electron microscopy image. Stress fields were extracted after 1800 s of cooling. At 0.001 m/s, increasing cladding power from 1500 to 3000 W raised the peak von Mises stress from approximately 356 to 433 MPa. At 2000 W, increasing scanning speed from 0.001 to 0.05 m/s reduced the peak from approximately 402 to 246 MPa. A separate regression dataset contained 1000 local stress records from 100 process combinations, with three process variables and a sampling-position index as predictors. Under record-level fivefold cross-validation, random forest achieved mean testing R2 values of 0.9458 for maximum principal tensile stress and 0.9845 for von Mises stress. CatBoost performed similarly. The two ensembles reproduced local FEA stresses at held-out records from the sampled fields.
No takes yet. Share an insight, caveat, or question.
Fan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: