Answers are grounded in this paper and cite their sources.
The corrosion behavior of T23 low−alloy steel was investigated in sulfate condensates relevant to coal–ammonia co-firing. Specimens underwent consecutive potentiodynamic polarization cycles at 30 °C in naturally aerated 5 wt.% H2SO4 and 5 wt.% NH4HSO4 solutions. Initially, the steel in NH4HSO4 had a lower corrosion current density estimated by Tafel extrapolation and a higher calculated polarization resistance than in H2SO4. The current-density ranking reversed by the 45th cycle. At the 50th cycle, the T23 low−alloy steel in NH4HSO4 showed a higher corrosion current density (NH4HSO4: 3.455 mA/cm2, H2SO4: 2.890 mA/cm2), a lower calculated polarization resistance, and greater specimen mass loss after cleaning. More precipitate was recovered from specimens exposed to NH4HSO4, although the solution contained 56.25% less Fe and 63.77% less Cr than H2SO4. The amount of Mn detected in solution was 117.1% higher. The lower amount of Fe in solution despite greater mass loss suggests differences in Fe partitioning between the electrolyte and solid corrosion products. X-ray diffraction and infrared spectroscopy supported the identification of FeSO4·4H2O and (NH4)2Fe(SO4)2·6H2O in precipitates recovered from H2SO4 and NH4HSO4, respectively. Electron microscopy showed less residual product coverage on the cleaned specimens exposed to NH4HSO4. Differences in corrosion-product composition and retention may help explain the reversal in corrosion ranking between the two electrolytes, which differ in acidity, sulfate speciation, and ammonium content.
No takes yet. Share an insight, caveat, or question.
Shin et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: