Answers are grounded in this paper and cite their sources.
Cr3+-activated near-infrared (NIR) phosphors are key for NIR phosphor-converted light emitting diodes (NIR pc-LED). While, the site occupancy of Cr3+ is one of the debates that have plagued researchers. Herein, Y2Mg2Al2Si2O12 (YMAS) with multiple cationic sites is chosen as host of Cr3+ to synthesize YMAS: xCr3+ phosphors. In YMAS, Cr3+ ions occupy simultaneously Al/SiO4 tetrahedral, Mg/AlO6 octahedral, and Y/MgO8 dodecahedral sites which form three luminescent centers named as Cr1, Cr2, and Cr3, respectively. Cr1 and Cr2 relate to an intermediate crystal field, with transitions of 2E→4A2 and 4T2→4A2 occurring simultaneously. As Cr3+ concentration increases, the 4T2→4A2 transition becomes more pronounced in Cr1 and Cr2, resulting in a red-shift and broadband emission. Cr3 consistently behaves a weak crystal field and exhibits the broad and long-wavelength emission. Wide-range NIR emission centering at 745 nm is realized in YMAS: 0.03Cr3+ phosphor. This phosphor has high internal quantum efficiency (IQE = 86%) and satisfying luminescence thermal stability (I423 K = 70.2%). Using this phosphor, NIR pc-LEDs with 56.6 mW@320 mA optical output power is packaged and applied. Present study not only demonstrates the Cr3+ multi-site occupancy in a certain oxide but also provides a reliable approach via choosing a host with diverse cationic sites and local environments for Cr3+ to achieve broadband NIR phosphors.
No takes yet. Share an insight, caveat, or question.
Li et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: