Answers are grounded in this paper and cite their sources.
Impact fracture behavior at low temperatures was investigated in medium manganese steel with bcc-fcc duplex microstructures. The impact energy was above 150 J (−80~20 °C) and the fractography showed dimples for inter-critical annealing at 630 °C (QHA) because of the high retained austenite stability and low martensite dislocation density. The impact energy was from 180 J (20 °C) to 60 J (−80 °C) and the fractography was intergranular for inter-critical annealing at 610 °C (QLA) because of the low stability of RA and carbides precipitated at the prior austenite grain boundaries. The impact energy was below 60 J (−80~20 °C) and the fractography showed cleavage for direct quenching (DQ) because of the high dislocation density of martensite.
No takes yet. Share an insight, caveat, or question.
Du et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: