Experimental analysis indicates micro-structure influences hydrogen embrittlement in austenitic stainless steels, suggesting grain refinement may improve resistance.
This study investigated the impact of micro-structure on hydrogen embrittlement (HE) in ultra-high strength Cr–Mn–N austenitic stainless steels fabricated via two distinct approaches: cold rolling (CR, deformation strengthening) and phase reversion annealing (fine-grained (FG), grain refinement). The CR specimen achieved a yield strength of 1.38 GPa but exhibited severe HE sensitivity due to strain-induced α′-martensite and dislocations acting as rapid hydrogen diffusion channels. In contrast, the FG specimen retained comparable strength (1.37 GPa) while demonstrating superior HE resistance, attributed to low-angle and Σ3 grain boundaries effectively suppressing H diffusion and inhibiting the propagation of cracks. Mechanistically, the CR specimen's high dislocation density (10.1 × 10 14 m −2 ) and α′-martensite content (26 vol.-%) facilitated hydrogen ingress (30.13 ppm total H), resulting in 46.4% elongation loss. Conversely, the FG specimen's refined micro-structure (1.2 μm grain size) with abundant Σ3 boundaries (0.29 μm μm −2 linear density) limited hydrogen penetration (16.98 ppm total H).
No takes yet. Share an insight, caveat, or question.
Ke et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: