Answers are grounded in this paper and cite their sources.
A novel strategy of introducing heterogeneous particles to promote dynamic precipitation is proposed for designing Mg-Bi alloys with high strength and excellent ductility. Through in-situ formation and extrusion, uniformly distributed trace Mg2Si particles are successfully obtained in the Mg-5Bi-3Al-0.4Si alloy. This significantly improves precipitation characteristics of nano Mg3Bi2 phases, as evidenced by reduced size and increased number density. Consequently, the Mg-5Bi-3Al-0.4Si alloy exhibits an increase in yield strength of 42 MPa, up to 371 MPa. Remarkably, introducing trace particles does not damage ductility, primarily due to the activation of non-basal slip and suppressed intergranular fracture tendency.
No takes yet. Share an insight, caveat, or question.
Li et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: