Answers are grounded in this paper and cite their sources.
Experimental study examines wear resistance enhancement in alloy coatings using Cr3C2, suggesting improved durability.
In an effort to acquire harder and more wear-resistant of FeCoCrNiMn high-entropy alloys, the Cr3C2 reinforced FeCoCrNiMn high-entropy alloy composite coatings were fabricated by laser cladding, and their microstructure, hardness and tribological properties were characterized. The results indicate that the coatings are composed of FCC matrix and Cr3C2 phase, and the addition of Cr3C2 enhances the microhardness (371.1–559.2 HV0.5). When paired with Si3N4 ceramic, the average friction coefficient first decreases from 0.77 to 0.59, and then increases to 0.64. When coupled with 440C steel, the average coefficient of friction first decreases from 0.71 to 0.50, and then rises to 0.62. Whereas, the addition of Cr3C2 carbide can critically improve the wear resistance, and the wear rate of the coatings paired with Si3N4 ceramic is always much lower than that of those paired with 440C steel. When paired with 440C steel, the minimum wear rate of 1.44×10−5 mm3/Nm can be achieved. When paired with Si3N4 ceramic, the minimum wear rate reaches 9.24×10−7 mm3/Nm (FeCoCrNiMn/20Cr3C2 coating), which is just 4.91% of the FeCoCrNiMn coating without Cr3C2 reinforcement. The superior wear resistance stems from cooperative effect of Cr3C2 enhancement and tribo-oxidization. The main wear mechanism against 440C steel is abrasive and adhesive wear, and the main wear mechanism against Si3N4 ceramic shifts from abrasive-adhesive to oxidative wear as the Cr3C2 content increases.
No takes yet. Share an insight, caveat, or question.
Huang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: