February 5, 20260 citationsOpen Access

Thermomechanical characterization of a cement mortar based on tyre granules

View Full Paper
APAbelim PASSOLITDTiambo Abbas DATCHOSSAEOE. Olodo

Key Points

  • The aim is to evaluate the thermomechanical characteristics of cement mortars incorporating tyre granules.
  • Formulated control mortar according to standard EN 196-1.
  • Added tyre granules at rates of 5%, 10%, 15%, and 20% to create different mortar formulations.
  • Performed thermal probe, compression strength, and three-point bending strength tests on the formulations.
  • Thermal conductivity decreases with the addition of tyre granules.
  • Flexural strength drops significantly from 5.95MPa (reference) to 1.31MPa (MT20).
  • Compressive strength decreases from 29.36MPa (MR) to 7.95MPa (MT20).
  • Optimal tyre granule content identified as 10% based on strength retention.

Abstract

Industrial waste management is a topical issue for both the present and the future. Current policies around the world encourage waste recovery as a means of managing waste. This study aims to recover tyre granules in construction materials. The goal is to determine the thermomechanical characteristics of cementitious mortars made from tyre granules. To achieve this, we formulated mortars in accordance with standard EN 196-1 for the control mortar. Tyre granules were then added to the control mortar at rates of 5%, 10%, 15% and 20% to produce formulations MT5, MT10, MT15 and MT20, with MR as the reference mortar. These formulations were tested using thermal probe, compression strength and three-point bending strength tests. The test results show that the addition of tyre granules leads to a reduction in thermal conductivity. Compressive and flexural strengths decrease with increasing tyre granule content. Flexural strength decreases from 5.95MPa for the reference mortar to 1.31MPa for the MT20 mortar. Compressive strength decreases from 29.36MPa for MR mortar to 7.95MPa for MT20 mortar. Compressive and flexural strengths indicate that 10% is the optimal rate for incorporating tyre granules into cement mortar.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

PASSOLI et al. (2025) studied this question.

synapsesocial.com/papers/6984358ff1d9ada3c1fb4829https://doi.org/10.5281/zenodo.18466948
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1Some Properties of a Cementitious Mortar Containing Granulated Rubber Waste and Brick Fillers: An Experimental Study, Mathematical Modeling and Optimization2024 · 3 citations
  2. 2Evaluation of Waste Tire Rubber as an Alternative Aggregate in Geopolymer Mortars2026 · 2 citations
  3. 3Evaluation of Mechanical and Microstructural Properties of Waste Tire Improved Cemented Clay2024 · 10 citations
  4. 4Mechanical properties of tire chip and cement stabilised red clay2024 · 2 citations
  5. 5Experimental investigation of mechanical and durability performance of high-performance rubberized mortar reinforced with steel fibers2026 · 1 citations