Recycling tyre-pyrolysis carbon as a cement substitute requires assessment of both bulk mortar and masonry interfaces. This study examined waste tyre carbon black (WTCB) at 0, 2.5, 5.0 and 7.5% cement replacement by mass without dispersing admixtures. Sand and effective water remained constant, with an effective water-to-total-powder ratio of 0.63. We measured fresh mortar flow and tested 180 specimens for mortar compression, direct tension, flexure, masonry prism compression, nominal diagonal shear and mortar–unit bond. Flow decreased from 113.06% to 105.94%. At 28 days, the 5.0% mixture had the highest mean mortar compressive strength (13.364 MPa), whereas the 7.5% mixture had the highest mean direct tensile strength (2.038 MPa). The 2.5% mixture had the highest mean prism strength on both test dates and the highest mean nominal diagonal shear strength at 28 days. It also showed the largest bond loss. At 28 days, all modified mixtures had lower flexural and bond means than the control, with bond losses of 17.5–46.2%. These differing rankings identify mortar–unit bond as an additional criterion for evaluating WTCB cement replacement alongside bulk strength. The results support further qualification of low replacement levels in the tested mortar–unit system.
No takes yet. Share an insight, caveat, or question.
Torres-Vásquez et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: