Demonstrates decreased electrical resistance in palladium films, suggesting improved hydrogen sensor performance.
We demonstrate a pronounced decrease in the electrical resistance of highly disordered palladium (Pd) films deposited under a high working Ar pressure using a compact film coating system. The resulting resistance change ratio of up to 1/335 is predominant among those reported previously. Film characterization suggests two primary mechanisms responsible for this significant resistance reduction: atomic force microscopy observation indicates improved electrical contacts among Pd grains, and X-ray diffraction measurement demonstrates hydrogenation-induced crystallization of Pd. These findings offer a simple scheme to enhance hydrogen sensor performance and can contribute to a more comprehensive understanding of the hydrogenation process in Pd.
No takes yet. Share an insight, caveat, or question.
Ikeda et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: