Demonstrates continuous production of expanded perlite in gypsum plaster, highlighting its sustainability.
• Continuous expanded perlite was produced with an updraft gasifier–cyclonic burner. • The best ASTM C35 density occurred at 1000°C. • The highest output occurred at 900°C with no agglomeration. • At 1000°C, <500 µm feedstocks passed ASTM C35 . • CO and particulate matter were acceptable, but NOx needs mitigation. This study demonstrates continuous production of expanded perlite for gypsum plaster using an integrated updraft gasifier–cyclonic burner system as a sustainable alternative to fossil-fuel heating. Burner temperature (900-1100°C) and feedstock particle size were evaluated for their effects on solids recovery, product morphology, ASTM C35 bulk density (96–192 kg m -3 ), mineralogy, and emissions. At 27.0 kg h -1 , 900°C gave the highest expanded-perlite yield (88.9% of feed) with no agglomeration, but produced an overall bulk density slightly below ASTM (91 kg m -3 ). At 1000°C, expanded-perlite yield decreased to 78.9% with minor agglomeration, while the overall bulk density met ASTM (143 kg m -3 ). At 1100°C, performance deteriorated severely, with usable yield dropping to 30.7% and agglomeration reaching 62.4% of collected solids. At 1000°C, feedstocks <500 µm satisfied ASTM C35 (143–179 kg m -3 ), whereas >500 µm exceeded the upper limit (290 kg m -3 ), indicating incomplete expansion under short flash residence time. X-ray diffraction under the recommended condition (1000°C, 250–500 µm) confirmed a predominantly glassy product (90.93 wt% amorphous; 3.07 wt% crystalline silica) with clay/mica and carbonates not detected. Particulate matter remained low and CO compliant at 900–1000°C, while nitrogen oxides require further mitigation.
No takes yet. Share an insight, caveat, or question.
Unsomsri et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: