Answers are grounded in this paper and cite their sources.
This research demonstrates enhanced damage tolerance in Cf/ZrB2-SiC-ZrC composites using a hybrid fabrication method.
A hybrid process combining slurry infiltration, low-temperature hot-pressing (HP), and precursor infiltration and pyrolysis (PIP) was developed to fabricate continuous C f /ZrB 2 -SiC-ZrC composites. Optimized HP at 1200 °C (40 MPa, 15 min) established a robust porous skeleton, which significantly reduced the subsequent PIP cycles to six, achieving a high bulk density of 2.93 g/cm 3 and low open porosity of 8.45 %. The optimal composite exhibited a flexural strength of 109.47 MPa. Notably, while the fracture toughness was moderate (3.77 MPa·m 1/2 ), the material demonstrated exceptional damage tolerance with a high work of fracture (578.98 J/m 2 ), attributed to extensive fiber pull-out and crack deflection mechanisms. After oxidation at 1500 °C, a continuous ZrO 2 -SiO 2 scale formed, allowing the composite to retain 30 % of its strength and maintain structural integrity. This work offers a strategic pathway for balancing densification efficiency and damage tolerance in UHTCMCs.
No takes yet. Share an insight, caveat, or question.
Qi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: