Answers are grounded in this paper and cite their sources.
The work-hardening properties of niobium single crystals grown by electron-beam zone-melting have been investigated over a wide range of purities, orientations, temperatures and strain-rates. Three stages of hardening are observed after the onset of plastic flow. The initial flow stress decreases with increasing purity, increasing temperature and decreasing strain-rate. In stage I the work-hardening rate θ1 is low (∼G/10 000 at room temperature) and increases with increasing temperature and decreasing strain-rate. The extent of stage I is a maximum at ∼273°K and stage I is absent for multiple slip orientations. In stage II the work-hardening rate θ11 is high (∼G/600) and is approximately independent of temperature above 295°K. θ11 is greater for multiple slip orientations and also increases with increasing purity. In stage III the work-hardening rate decreases continuously until fracture. Stage III is more prominent at high temperatures and the stress at the onset of Stage III, τ111, decreases with increasing temperature. Slip-line observations show that slip occurs initially on (011) planes and that in stage II bands of secondary slip occur. The nature of the slip lines observed in stage I is compatible with the view that some cross-slip of screw dislocations occurs and that edge dislocations slip much further than screws.
No takes yet. Share an insight, caveat, or question.
Mitchell et al. (1963) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: