A picosecond pump-probe technique is used to measure the room-temperature thermal conductivity κ and longitudinal sound velocity cl of amorphous diamond (a-D) and diamondlike carbon (DLC) thin films. Both κ and cl were found to decrease with film hydrogen content. Depending on the film deposition technique, κ is in the range 5–10×10−2 W cm−1 K−1 for a-D, and 3–10×10−3 W cm−1 K−1 for DLC. Values of cl were found to be in the range 14–18×105 cm s−1 for a-D, and 6–9×105 cm s−1 for DLC.