This is the authors' abstract. We don't add key points for this paper.
Radiant exposures delivered by the various irradiation protocols were between 4.5-30.3 J/cm². Short exposure times from MONET-1 s and PW-3 s delivered the lowest radiant exposures (4.5 and 5.2 J/cm², respectively) and produced the lowest ΔT and DC. The longer exposure times in the standard modes of PW-20 s, S10-20 s, and MONET-3 s produced the highest Tmax, ΔT, and DC for both composites. The ΔT range among composites at different depths varied significantly (31.7-49.9 °C). DC of TPF ranged between 30-65% and in EVO between 15.3-56%. TPF had higher Tmax, ΔT for all depths and DC compared to EVO, across the LCU protocols (p < 0.05), except for PW-20 s and MONET-3 s. The coronal part of the restorations (1-2 mm) had the highest ΔT. There was a positive correlation between ΔT and DC at 4-mm depth after 120 s SIGNIFICANCE: Longer, or standard, exposure times of the LCUs delivered greater radiant exposures and had higher DC and ΔT compared to shorter or high-irradiance protocols. The fast photo-polymerised RBC had comparatively superior thermal and conversion outcomes when it received a high irradiance for a short time (1-5 s) compared to the conventional Bulk-Fill RBC.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Thanoon et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: