Investigates oxidation resistance in (Zr,Ti,W)C-based ceramics, suggesting improved performance for nuclear fusion applications.
This study systematically investigates the high-temperature oxidation behaviour of (Zr,Ti,W)C-Me x B y multiphase ceramics fabricated by spark plasma sintering, focusing on their performance in static air at 1000°C – 1100°C (operating temperature range for divertor components in nuclear fusion devices). The oxide layers consist predominantly of t-TiO 2 , m-ZrO 2 and (Ti, Zr)O 2 /(Zr,Ti)O 2 solid solutions. At 1000°C, oxidation follows parabolic kinetics, suggesting diffusion-controlled growth. At 1100°C, linear kinetics prevail as enhanced volatilisation of WO 3 and B 2 O 3 leads to porous microstructures. The outer oxide layer develops voids due to WO 3 sublimation, while the inner layer remains dense owing to B 2 O 3 filling the pores and cracks. The multiphase oxide structure, comprising (Zr,Ti)O 2 and (Ti,Zr)O 2 solid solutions along with dispersed ZrO 2 and TiO 2 particles, substantially enhances the oxidation resistance. The incorporation of ZrB 2 significantly increases the apparent activation energy of oxidation from 13.3641 kJ/mol (TW) to 47.4178 kJ/mol (TW60ZB), representing a 355% improvement in oxidation resistance. The key mechanisms include prolonged oxygen diffusion paths due to low-diffusivity ZrO 2 regions, grain boundary pinning by interphase boundaries and microstress fields at TiO 2 /ZrO 2 interfaces that deflect microcracks. These results demonstrate the promising potential of (Zr,Ti,W)C-Me x B y ceramics for high-temperature applications such as nuclear fusion divertor components.
No takes yet. Share an insight, caveat, or question.
Zhuang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: