Shows improved dopant activation in epitaxial silicon, suggesting a new method for enhanced conductivity.
As silicon devices continue to scale, source–drain series resistance has become a critical limitation, which has motivated the development of heavily doped n-type silicon formed by in situ epitaxial doping. However, phosphorus, the most widely used n-type dopant, exhibits limited electrical activation at high concentrations due to the formation of phosphorus–vacancy complexes. In this work, we report the first experimental investigation of phosphorus–antimony (P–Sb) co-doping in epitaxial silicon grown by ultrahigh-vacuum chemical vapor deposition using a metal–organic antimony precursor. We show that simultaneous P–Sb co-doping is ineffective in the heavily doped regime, whereas a sequential co-doping strategy that introduces phosphorus during the initial growth stage followed by antimony effectively enhances dopant activation. The optimized sequentially co-doped film achieved a carrier concentration of 1.06 × 1020 cm−3, a Hall mobility of 71.25 cm2 V−1 s−1, and a conductivity of 1208 Ω−1 cm−1. The efficiency of the dopant activation evaluated using areal carrier and dopant densities from Hall-effect measurements and secondary ion mass spectrometry increased from 16.6% for phosphorus-only doping to 63.9% for sequential co-doping. Subsequent oxygen-ambient rapid thermal annealing suppressed phosphorus out-diffusion and reduced sheet resistance from 275 to 45.1 Ω/sq, among the lowest values reported for heavily doped n-type silicon. These results demonstrate that sequential P–Sb co-doping enabled by a metal–organic antimony precursor provides an effective and scalable approach to grow highly conductive n-type silicon epitaxial layers for advanced source–drain engineering.
No takes yet. Share an insight, caveat, or question.
Jeong et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: