Phase evolution and magnetic properties of melt-spun (Fe0.675Pt0.325)100−xBx (x=12–20) nanocomposite ribbons are investigated. For those ribbons spun at 45m∕s, followed with a 500°C isothermal annealing for 1–6h, the boron addition not only promotes disorder to order (γ→γ1) transformation but also leads to the formation of different kinds of Fe-borides. Pt exhibits a strong affinity to Fe during thermal processes in forming magnetically hard γ1(FePt) phase, leaving excess Fe to interact with B in forming Fe2B, Fe3B, or FeB. For x=12–18, all ribbons are composed of one hard phase, γ1-FePt, and three soft phases, γ-FePt, Fe2B, and Fe3B. But FeB also coexists for x=20. Through the exchange-coupling interaction between nanoscale γ1-FePt and multiple soft phases, record of magnetic properties of Br=9.4kG, Hci=7.5kOe, and (BH)max=14.0MGOe has been successfully developed in isotropic (Fe0.675Pt0.325)84B16 ribbons, where the reduced remanence ratio (σr∕σ12kOe) is as high as 0.86.
No takes yet. Share an insight, caveat, or question.
Chang et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: