Answers are grounded in this paper and cite their sources.
A P-E hysteresis loop is observed in polyvinylidene fluoride film with a spontaneous polarization of 8 μcoul/cm2at 140°C. The spontaneous polarization, obtained by the integration of the pyroelectric current, decreases with increase in temperature. The pyroelectric current shows a minimum at the solid-to-glass transition temperature (-40°C). The dielectric constant at 25°C, measured at -.003 Hz, is -1000, or two orders of magnitude larger than the value measured at 50 Hz. The switching current above 120° C has the form Jmax = JoEne - α/kT with n varying from 0.7 to 1.6 and α equal to 0.65 eV. The inverse switching time shows a similar dependence on field and temperature, with an activation energy of 1 eV. The long switching time, of the order of several minutes at 150°C, suggests that polarization reversal is associated with the rotation of the long chain molecules by the applied field.
No takes yet. Share an insight, caveat, or question.
P. Buchman (1973) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: