Answers are grounded in this paper and cite their sources.
We try to obtain stable supercontinuum (SC) generation with broad bandwidth under relative simple pump conditions. We use a 1.3-m-long highly nonlinear tellurite microstructured fiber and pump it by a 15 ps 1064 nm fiber laser. One segment of the fiber is tapered from a core diameter of 3.4 μm to 1.3 μm. For the first time five-order stimulated Raman scatterings (SRSs) are observed for soft glass fibers. SC covering 730-1700 nm is demonstrated with the pump-pulse-energy of several nJ. The mechanisms of SC broadening are mainly SRS, self-phase modulation (SPM) and cross phase modulation (XPM). The tapered segment has two advantages. Firstly it increases the nonlinearity of fiber by several times. Secondly, it acts as a compensation for the dispersion of the untapered segment, and mitigates the walk-off between pump pulse and SRS peaks.
No takes yet. Share an insight, caveat, or question.
Liao et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: