Explores compressive strength in mortar with alkali bypass dust, highlighting waste valorization benefits.
This study investigates the use of Alkali Bypass Dust (ABD), a cement kiln waste, as a supplementary cementitious material in mortar. Direct ABD incorporation reduced workability and strength. A dual-modification strategy employing a water reducer (WR) and silica fume (SF) was implemented. Mortars with 0–50% cement replaced by ABD were tested, with and without modifiers. Results showed that WR effectively restored workability and improved early strength, while SF enhanced long-term performance through pozzolanic reactions. A synergistic effect in ternary blends (ABD + WR + SF) yielded 28-day compressive strength at 50% ABD replacement comparable to the control (49.9 MPa). Statistical analysis via Response Surface Methodology confirmed that material interactions, not individual amounts, primarily govern strength development. All models are significant where R2 value is higher than 0.80. The statistically validated models can be used to optimize the mix proportions for desired compressive and flexural performance. The study concludes that optimized blends with 30–50% ABD are viable for non-structural applications, offering a sustainable pathway for waste valorization and reduced cement consumption.
No takes yet. Share an insight, caveat, or question.
Alturki et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: