Shows improved corrosion resistance in Alloy 600, suggesting ULP treatments enhance durability.
The effect of underwater laser peening (ULP) on the localized corrosion resistance of Alloy 600 in deaerated 3.5 wt.% NaCl solution was investigated through a comparative study of four surface conditions: polished, heavy grinding (HG), single-pass ULP (ULP(x1)), and two-pass ULP (ULP(x2)). ULP was performed at a beam intensity of 4∼5 GW/cm 2 and a pulse density of 64 pulses/mm 2 without an ablative layer. While single-pass ULP provided initial improvements over the HG surface, the two-pass ULP treatment resulted in a superior electrochemical response, characterized by a significant noble shift in the breakdown potential ( : from −95 mV to +216 mV vs. SCE) and a marked increase in charge-transfer resistance ( > 10,000 kΩ·cm 2 ). Cross-sectional analyses revealed that the two-pass treatment facilitated the formation of a more continuous Cr-rich surface oxide and the reconstruction of a less porous recast layer. These features act as an effective barrier, thereby suppressing metastable pitting and stabilizing the passive state. It is found that Cr-rich oxide continuity and recast-layer physical integrity are the primary governing factors controlling the electrochemical corrosion behavior of ULP-treated nickel-based alloys in chloride environments.
No takes yet. Share an insight, caveat, or question.
Bai et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: