Answers are grounded in this paper and cite their sources.
Compares construction processes' effects on alloy properties, indicating method impacts performance.
Ti–6Al–2Sn–4Zr–2Mo (Ti-6242), a near-α titanium alloy designed for high-temperature aerospace applications, was fabricated using electron beam powder bed fusion (EB-PBF), laser powder bed fusion (L-PBF), and laser powder directed energy deposition (LP-DED). A systematic comparison was conducted to elucidate the relationships between processing route, defect population, microstructure, mechanical response, and corrosion behavior. X-ray computed tomography revealed distinct porosity characteristics, with relative densities of ~99.95%, 99.97%, and 99.99% for L-PBF, EB-PBF, and LP-DED, respectively. L-PBF samples exhibited finer but more numerous lack-of-fusion and keyhole-type pores, whereas EB-PBF showed larger, predominantly gas-induced porosity. LP-DED produced the lowest defect severity with reduced pore size and volume fraction. The superior density of LP-DED is attributed to larger, more stable melt pools that facilitate gas escape, whereas the higher defect count in L-PBF stems from keyhole instabilities and lack-of-fusion associated with its smaller beam spot and higher scan speeds. Microstructural analysis revealed that while columnar prior-β grains (9–53 μm wide) were common to all processes, the final microstructure characteristics was strongly process-dependent: L-PBF resulted in refined acicular α′ martensite with lath widths below ~0.4 μm due to rapid cooling, EB-PBF produced coarser α laths (~0.5–0.8 μm) within a basketweave morphology owing to elevated build temperatures, and LP-DED exhibited the coarsest α+β microstructure with lath widths exceeding 1 μm. These variations are driven by the extreme cooling rates in L-PBF which trigger a displacive martensitic transformation, contrasted by the in-situ thermal aging of the EB-PBF heated powder bed and the high heat input of LP-DED, which promote diffusional growth of alpha laths. Correspondingly, nanoindentation hardness decreased from ~5.24 GPa (L-PBF) to ~5.12 GPa (EB-PBF) and ~4.87 GPa (LP-DED). This trend correlates with the Hall-Petch strengthening effect derived from refined lath scales and the significantly higher dislocation density observed in L-PBF samples due to severe thermal gradients. Electrochemical testing in 3.5 wt.% NaCl solution indicated superior corrosion resistance for L-PBF and LP-DED, with corrosion current densities approximately one order of magnitude lower than EB-PBF. The reduced performance of EB-PBF is attributed to the presence of larger LOF defects and the simultaneous presence of distinct alpha and β phases; this heterogeneous phase distribution likely facilitates the formation of micro-galvanic cells, accelerating localized corrosion. These findings highlight the critical role of additive manufacturing strategy in tailoring the microstructure and performance of Ti-6242 for demanding structural applications.
No takes yet. Share an insight, caveat, or question.
Behjat et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: