Phase transformation kinetics are analyzed in Sr-hexacelsian towards celsian, suggesting implications for material properties.
The isothermal transformation of Sr-hexacelsian to celsian in sintered bodies having chemical composition xSrO·Al2O3·2SiO2 (x = 1.0, 1.1 and 1.2) was analyzed using X-ray diffraction and JMA kinetics. All compositions showed rapid initial transformation followed by strong deceleration, and excess SrO accelerated the reaction. JMA plots exhibited two linear regions, indicating a mechanism change caused by crack formation at the advancing transformation front. Significant volume contraction, enhanced at high temperature due to thermal-expansion mismatch, generated internal stresses that promoted cracking and constrained later-stage growth. The Avrami index increased from 1.5 to about 2 with temperature, consistent with a shift from one-dimensional to two-dimensional growth. High activation energies (833–934 kJ/mol) were attributed to stress interactions between anisotropic hexacelsian grains.
No takes yet. Share an insight, caveat, or question.
Kobayashi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: