The purpose of this work is to clarify the transformation mechanism from hexacelsian to celsian and the thermal expansion properties of celsian solid solutions (Ba 1-x Sr x Al 2 Si 2 O 8 , x = 0-1.0)using high-temperature powder X-ray diffraction and dilatometry of sintered polycrystals.Hexacelsian polycrystals were prepared from BaCO 3 , SrCO 3 and finely purified kaolin powder (Al 2 O 3 •2SiO 2 •2H 2 O) by heat-treatment at 950-1400°C.Sr-hexacelsian polycrystals transformed to celsian via nucleation and growth from inner to surface to develop cracks at surface at 1100 -1200°C.Single phase of celsian polycrystals in composition of Ba 1-x Sr x Al 2 Si 2 O 8 , x = 0 -0.8) were prepared by heat-treatment at 1400°C for 1 hour and their dilatometric thermal expansion coefficient (TEC) were almost 4.0 -4.2x10 -6 /°C from 25 to 900°C.On the other hand, average TEC of unit cell of celsian measured by high temperature X-ray diffraction were lower than the values of dilatometry and increased from 3.0x10 -6 /°C to 3.8x10 -6 /°C with the Sr content.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kobayashi et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: