Shows improved capacity in sodium-ion battery cathodes, indicating better performance for energy storage.
The aim of this article was to improve the solid-phase synthesis of Na3V2(PO4)3/C composite for sodium-ion battery cathode materials using an innovative technique for creating a protective reducing atmosphere, which is formed by incomplete oxidation of carbon fiber during annealing. The resulting Na3V2(PO4)3 phase has a rhombohedral structure of a sodium superionic conductor (NASICON) with particle sizes ranging from 0.5 to 20.0 μm. The encapsulation of Na3V2(PO4)3 granules with a carbon coating leads to a maximum specific capacity of 112.3 mAh g−1 at a charge–discharge rate of C/5 (22.4 mA g−1). After 200 charge–discharge cycles, the synthesized composite demonstrated a specific discharge capacity degradation of 0.107% per cycle. The apparent diffusion coefficients of Na+ ions in the resulting Na3V2(PO4)3/C composite were measured and found to be 5.87 × 10−11 and 4.60 × 10−11 cm2 s−1 for deintercalation and intercalation, respectively.
No takes yet. Share an insight, caveat, or question.
Sidorov et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: