Investigates localized corrosion dynamics in carbon steel, suggesting new inhibition strategies.
Internal localized corrosion of carbon steel pipelines severely threatens the service safety of oil and gas transportation facilities in CO 2 -containing aqueous environments. In this work, the corrosion evolution and localized corrosion initiation mechanisms of carbon steel in CO 2 –Cl − –HCO 3 − coexisting environments were systematically investigated under varying temperatures and HCO 3 − concentrations. The results demonstrate that the initiation of localized corrosion is primarily attributed to the formation of loose and porous FeCO 3 films, which fail to block the permeation of aggressive Cl − and expose the steel substrate to continuous corrosion. In contrast, the synergistic effect of elevated temperature and appropriate HCO 3 − concentration significantly improves FeCO 3 supersaturation and promotes the formation of dense, uniform, and protective FeCO 3 films, which effectively isolate the substrate from corrosive media and inhibit localized corrosion. Furthermore, this study quantitatively clarifies the optimal matching relationship between temperature and HCO 3 − concentration for the growth of high-quality protective FeCO 3 films. The findings provide fundamental mechanistic insights and practical guidance for the targeted regulation of HCO 3 − to mitigate localized corrosion of carbon steel in CO 2 -saturated oil and gas production systems.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: