Answers are grounded in this paper and cite their sources.
Evaluates hydrogen production and dye degradation in antimony sulfide films, indicating effectiveness with palladium.
This study presents a novel galvanic deposition method to create antimony sulfide thin films on FTO glass. The presence of palladium as a top layer on the surface of Sb 2 S 3 (designated as Sb 2 S 3 :Pd) promotes hydrogen production and dye degradation. Four differently treated Sb 2 S 3 films were studied. In neutral buffer medium, maximum efficiency related to water splitting for hydrogen evolution was observed for the annealed Sb 2 S 3 :Pd films, displaying a low onset potential of −116 mV and a Tafel slope of 64 mV/decade. The inclusion of Pd boosts the HER performance, which exhibits a current density of 10 mAcm −2 at a comparatively lower overpotential of −204 mV with significant stability. Sb 2 S 3 :Pd films also demonstrated improved dye degradation capability in comparison to Sb 2 S 3 films without Pd.
No takes yet. Share an insight, caveat, or question.
Ahamed et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: