Investigates mechanical strength and thermal resistance in mortar with stone dust, indicating sustainable construction benefits.
The increasing scarcity of natural sand (NS) and the environmental impact of quarrying necessitate the exploration of sustainable alternatives to fine aggregate in construction. This study investigates the mechanical performance and thermal resistance of cement mortar incorporating stone dust (SD) as a partial replacement of NS. Mortar mixes were prepared with 0%, 15%, 30%, 45%, and 60% SD replacement by mass, while maintaining a constant cement‐to‐fine‐aggregate ratio of 1:3 and an initial water‐to‐cement ratio of 0.5. Compressive strength was evaluated under ambient conditions and after exposure to elevated temperatures of 100°C, 200°C, 300°C, 500°C, and 700°C. Mass loss was measured to assess thermal degradation, and microstructural characteristics were examined using scanning electron microscopy and energy‐dispersive X‐ray spectroscopy. The results show that the inclusion of 15% SD produced the highest compressive strength of 32.03 N/mm 2 , a 15.7% increase over the control mix. Beyond 30% replacement, strength decreased due to increased water demand and reduced paste–aggregate bonding. Thermal exposure caused progressive strength degradation in all mixes; however, SD15 exhibited superior retention of residual strength and lower mass loss than the control specimen. Microstructural observations confirmed a denser matrix and improved interfacial bonding at moderate SD content, driven by filler effects and a refined pore structure. Based on overall performance, 15% SD replacement is identified as the optimum dosage for improving the strength and thermal stability of cement mortar.
No takes yet. Share an insight, caveat, or question.
Kumar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: