This study investigates the crack resistance of rice husk ash (RHA)–incorporated SFRSCC, with RHA contents from 2.50% to 15.00% and water–cement ratios (W/C) from 0.35 to 0.50. ENDB samples were tested under mode I, mode III, and combined III/I loading to enable a comprehensive fracture-resistance assessment. Results show that increasing W/C from 0.35 to 0.50 raises workability by 50.71%, while the same tests with RHA reduce it to about 15.00%. Moreover, for each increment of RHA from 2.50% to 15.00% within a 0.40–0.50 W/C range, maximum load improves by 62.35%. At W/C = 0.35, 15.00% RHA slightly lowers compressive strength by 2.83% and UPV by 2.43. In contrast, at W/C = 0.40 and 0.50, strengths rise by 27.41% and 27.61%, indicating improved microstructure and pozzolanic activity. The greatest fracture toughness under mode I occurs for a mix with 7.50% RHA and W/C = 0.35, 25.42% above the reference; at higher W/C, increases reach up to 97.51%. The ANN model predicts fracture toughness with R = 0.993 and errors under 15%. SHAP analysis identifies loading condition, W/C, and UPV as dominant influences on toughness. Overall, optimizing RHA and W/C enhances SFRSCC fracture toughness for real projects.
No takes yet. Share an insight, caveat, or question.
Sun et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: