A method was developed to identify unstable mixes with the help of Superpave gyratory data. The basis of this method is that the primary difference in behavior of a stable mix and an unstable mix is that a stable mix gains in strength with densification and retains it through further compaction and ultimately resists lowering of voids below a particular value, whereas an unstable mix initially gains in strength but loses it beyond a certain densification point and becomes susceptible to shear failure. Hence it is proposed that the strength of a mix be evaluated at two void levels: at 5 percent, where a mix is expected to have an increased shear strength compared with postconstruction voids, and at 2 percent, where a well-performing mix should have an increased or at least similar shear strength compared with shear strength at 5 percent, and where an unstable mix is expected to have a reduced shear strength compared with shear strength at 5 percent voids. U.S. Army Corps of Engineers and Superpave gyratory compaction data were obtained for five mixes from wearing courses, and the data were evaluated with the help of in-place rutting data. The gyratory ratio, a ratio of the number of gyrations required to achieve 2 percent voids and 5 percent voids, was found to be suitable for characterizing hot-mix asphalt. Theoretical calculations and in-place rutting data show that a gyratory ratio of 4 can be used to differentiate between stable and unstable mixes—mixes with a gyratory ratio less than 4 can be expected to be unstable.
No takes yet. Share an insight, caveat, or question.
Rajib B. Mallick (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: