Answers are grounded in this paper and cite their sources.
Objectives: To assess the shear bond strength (SBS) of chairside computer-aided design and computer-aided manufacturing (CAD-CAM) blocks to dentin subjected to simulated gastric erosion when cemented with self-etch and self-adhesive resin cements. Materials and Methods: One hundred eighty dentin samples were assigned to two groups: sound and eroded dentin. In the eroded dentin group, samples were eroded with HCl (0.01 M, pH 2, 2 min) and stored in artificial saliva for 60 min then, brushed using a power brush (2N, 15 s). This cycle was repeated three times. CAD-CAM blocks (3x3x3 mm3, n=15/group) of Lava Ultimate (LU), Vita Enamic (VE), and Vita Suprinity (VS) were cemented to sound and eroded dentin with self-etch Multilink N (MN) and self-adhesive RelyX U200 Automix (RU) resin cements. SBS was measured after 24 hours. The failure mode was assessed by using a stereomicroscope. Data was analyzed with 3-way ANOVA and Bonferroni correction (p˂0.05). Results: The SBS was significantly affected by the main factors: tooth structure (p=0.011), resin cements (p˂0.001), and CAD-CAM blocks (p=0.001). When LU was cemented with RU to sound dentin, a higher SBS was obtained compared to eroded dentin (p=0.001). MN revealed significantly higher SBS than RU (p<0.05). When using MN in sound dentin LU showed lower bond strength than VE and VS (p<0.05). The predominant failure mode was mixed for all groups. Conclusions: It was determined that the bond strength of dentin was affected by simulated gastric erosion. The use of Multilink N resin cement in both sound and eroded dentin can be recommended. For a reliable bond to eroded dentin, selection of the proper cement system and material type are necessary.
No takes yet. Share an insight, caveat, or question.
Naiboğlu et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: