Answers are grounded in this paper and cite their sources.
The pulsed and CW laser performance of a range of titanium sapphire laser crystals is reported. Titanium ion concentration in the crystals ranged from 0.07 at.% to 0.25 and 0.41 at.% for some recently developed heavily doped crystals. Values of the crystal figure of merit lay between 30 and 220. Threshold, slope efficiency, tunability, and temporal response are assessed. Comparisons are made with the predictions of a simple rate equation model.
No takes yet. Share an insight, caveat, or question.
McKinnie et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: