Answers are grounded in this paper and cite their sources.
Measurements of transmission loss coefficients in AgGaSe(2) at 2.1 microm ranged from 0.012 to 0.072 cm(-1). Energy density, not peak-power density, proved to be the determining factor in AgGaSe(2) damage threshold. Coated-surface damage thresholds originally were found to be in the 1.1-2.5-J/cm(2) region by using 180-nsec laser pulses, but damage thresholds as high as 3.5 J/cm(2), with a 3 J/cm(2) average, were measured in coated samples with improved surface quality.
No takes yet. Share an insight, caveat, or question.
Ziegler et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: