Answers are grounded in this paper and cite their sources.
Half-ring waveguides (5 μm width, 185 μm radius) fabricated by liquid-phase expitaxial growth of Ga1−xAlxAs and GaAs layers over preferentially etched channels in GaAs substrates were made to lase by optical pumping with a N2 laser (λ=3371 Å) at 77 °K. The half-ring lasers had a threshold of about 2×104 W/cm2; a bending loss per radian αc<1.5 cm−1; strong TE polarization; and a well-defined circumferential mode structure: Δλ≃1.07 Å at λ=8280 Å for a 580-μm-long cavity. Straight guides of similar profile to the circular guides were made to lase for comparison. A calculated 0.5-Å mode broadening due to transient heating during the pump laser pulse accounts for the observed lasing spectra.
No takes yet. Share an insight, caveat, or question.
Botez et al. (1976) studied this question.