Answers are grounded in this paper and cite their sources.
Propagation losses are calculated for magnetostatic surface waves in slabs of YIG and LiFe5O8. A phenomenological (Gilbert) magnetic damping is assumed and known magnetic parameters are used. The propagation loss factor L (dB/μsec) is calculated as a function of frequency. At high frequencies we find that L is proportional to frequency with a slope of 4π(76.4λ/γ2M), where λ is the damping parameter, γ is the gyromagnetic ratio, and M is the magnetization. At low frequencies, L approaches a limiting value of 4π(76.4λ/γ). The quantity L is independent of slab thickness, although both loss and delay time are functions of thickness for a given slab length. Our calculated L is in reasonable agreement with recent measurements. As expected, magnetic anisotropy has a greater effect on L for LiFe5O8 than for YIG.
No takes yet. Share an insight, caveat, or question.
Vittoria et al. (1974) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: