Answers are grounded in this paper and cite their sources.
The fabrication process and the head material properties for shielded magnetoresistive heads with planarized lower shields using a tri-layered MR element are described in detail. Applying the etch-back process with low molecular weight polystyrene and CF/sub 4//O/sub 2/ reactive ion etching, the residual step height for a lower shield is dramatically decreased to less than 5% of the initial step height. The tri-layered MR element consists of an MR layer, a magnetic separation layer (MSL), and a soft adjacent layer (SAL). 40-nm thick Ni/sub 81/Fe/sub 19/ (wt.%) films were deposited by evaporation for use as an MR layer. Evaporated Ti MSL thickness was experimentally determined to be 20 nm. Amorphous Co/sub 82/Zr/sub 6/Mo/sub 12/ SAL films exhibited preferable magnetic properties as an SAL material. The fabricated shielded MR heads, using the tri-layered MR element with these NiFe, Ti, and CoZrMo films, provide superior capability to realize high recording density.>
No takes yet. Share an insight, caveat, or question.
Yamada et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: