Fabrication and annealing properties of MgO/CoFeB/MgO on its perpendicular magnetic anisotropy (PMA) were evaluated. The double CoFeB-MgO structure was formed by removing the capping Ta layer of the initial Ta/CoFeB/MgO structure, followed by a second MgO layer and a W capping layer deposition. A decrease in magnetization saturation ( M s ) due to the formation of a magnetic dead layer was recovered by annealing at over 250 °C, exceeding the initial M s values. From the CoFeB thickness dependency, 1.8 times higher interfacial anisotropy ( K i ) was obtained with a double CoFeB-MgO interface, thereby preserving perpendicular magnetic anisotropy (PMA) up to a CoFeB thickness of 1.7 nm. A PMA film with a thicker film thickness is advantageous to obtain a high thermal stability (Δ) for scaled non-volatile magnetic memory devices.