Refractive indexes of ZnSe, ZnTe, and CdTe were obtained from prism refraction data and are reported for a series of wavelengths from 2.5 μ to the short-wave transmission limits set by the band gaps. The results were fitted with the standard formula: n2=A +[Bλ2/(λ2−c2)] where n is the refractive index and λ is the wavelength in microns. For ZnSe the best values of the parameters are A=4.00, B=1.90, and c2=0.113; for ZnTe, A=4.27, B=3.01, and c2=0.142; and for CdTe, A=5.68, B=1.53, and c2=0.366. Possible causes for the discrepancies between the present results and earlier data are discussed.
No takes yet. Share an insight, caveat, or question.
D. T. F. Marple (1964) studied this question.