The crystal and amorphous orientation functions of polypropylene (PP) and high-density polyethylene (HDPE) sheets, stretched by the roller-drawing technique, were measured by means of infrared dichroism and visible-ultraviolet dichroism. The molecular chains in the crystalline and amorphous regions lined up parallel to the draw direction in the roller-drawing process. At higher draw ratio (λ > 7–13), the crystal orientation function approached a constant value, whereas the amorphous orientation function increased monotonically with draw ratio. Film tilting measurements revealed that the deviation from symmetric uniaxial orientation was small for the roller-drawn HDPE and PP sheets. In the case of HDPE, the fraction of—GTTG—,—4TG—, and—GG—sequences decreased, and that of the trans-rich sequences increased in the roller-drawing process. These changes were interpreted in terms of the Peterlin model. The orientation function calculated from visible-ultraviolet dichroism decreased greatly with decreasing length of solute (dye) molecules. The reasons for this phenomenon are discussed.
No takes yet. Share an insight, caveat, or question.
Kaito et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: