The temperature dependence of the specific saturation magnetization of barium and strontium ferrite powders after milling in an attrition mill has been investigated at temperatures between -195°C and the Curie temperature of the ferrites. The experimental results show that the specific saturation magnetization decreases with increasing milling time and that a second, presumably soft-magnetic phase occurs during milling which vanishes during annealing of the powders. The influence of lattice defects introduced by the milling process is discussed.