The binary mixtures of the substance magnified image providing cholesteric phase exhibit a chiral SmC* phase for certain concentration and temperature range. This phase was verified to be ferroelectric. The temperature dependences of the spontaneous polarization and the coercive field were determined for three concentrations. The pitch of the helical structure is approximately indirectly proportional to the molar concentration of the cholesteric substance and varies from 3 μm to about 25 μm in the concentration range from 20 mol% to 5 mol% of the cholesteric substance. For the lower concentrations the sample is unwound in planar samples due to the surface anchoring. Two possible unwound planar configurations can be switched by electric field.