Answers are grounded in this paper and cite their sources.
We have systematically investigated the influence of different bonding parameters on void formation in a low-temperature adhesive bonding process. As a result of these studies we present guidelines for void free adhesive bonding of 10 cm diameter wafers. We have focused on polymer coatings with layer thicknesses between 1 µm and 18 µm. The tested polymer materials were benzocyclobutene (BCB) from Dow Chemical, a negative photoresist (ULTRA-i 300) and a positive photoresist (S1818) from Shipley, a polyimide (HTR3) from Arch Chemical and two different polyimides (PI2555 and PI2610) from DuPont. The polymer material, the bonding pressure and the pre-curing time and temperature for the polymer significantly influence void formation at the bond interface. High bonding pressure and optimum pre-curing times/temperatures counteract void formation. We present the process parameters to achieve void-free bonding with the BCB coating and with the ULTRA-i 300 photoresist coating as adhesive materials. Excellent void-free and strong bonds have been achieved by using BCB as the bonding material which requires a minimum bonding temperature of 180 °C.
No takes yet. Share an insight, caveat, or question.
Niklaus et al. (2001) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: