Answers are grounded in this paper and cite their sources.
TiC x films were deposited by atomic layer deposition using tetrakis–neopentyl–titanium [ Ti ( CH 2 C ( CH 3 ) 3 ) 4 ] and H 2 plasma as the precursor and reactant, respectively. The growth of the rock‐salt–structured TiC x films was confirmed by X ‐ray and electron diffraction. The C ‐to‐ Ti ratio determined by Rutherford backscattering spectrometry was ~0.52 and the film resistivity was as low as ~600 μΩ cm with a high density of 4.41 g/cm 3 . The step coverage was approximately 90% over the trench structure (top opening diameter of 25 nm) with an aspect ratio of ~4.5.
No takes yet. Share an insight, caveat, or question.
Hong et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: