MgO thin films are deposited by chemical vapor deposition from the precursor magnesium N,N-dimethylaminodiboranate, Mg(H3BNMe2BH3)2, and water at a substrate temperature of 270–350 °C. Highly conformal coatings with 98% step coverage in trenches of aspect ratio 9 are obtained at a substrate temperature of 270 °C and a growth rate of 7.5 nm/min, most notably through the use of a forward-directed flux, in which some of the precursor molecules travel ballistically down the recessed feature, strike the bottom, and are scattered there to create a virtual source. The deposition conditions can also be adjusted to afford a growth rate up to 200 nm/min with reduced conformality. Most of the films have a dense and column-free microstructure with low surface roughness; the film density, measured by a combination of Rutherford backscattering spectrometry and scanning electron microscopy, is 82%–86% of bulk. Films grown on Si substrates have good adhesion and a low coefficient of friction (∼0.1) in nanoscratch measurements. The refractive index of the films is slightly lower than that of bulk MgO, consistent with the reduced physical densities. Depending on the growth conditions, the C content in the films varies between 0.7 and 6 at. %, and the B content ranges from 1 to 16 at. %. B in the film is present in the B2O3 chemical state; after subtracting the O content in B2O3, the O/Mg ratio = 1.02 in the MgO matrix. A film grown at a temperature of 270 °C and a growth rate of 6 nm/min has a dielectric constant of 9.5 and a breakdown strength of 6 MV/cm.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Talukdar et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: